User Tools

Site Tools


cressington_sputter_coater_208hr

Differences

This shows you the differences between two versions of the page.

Link to this comparison view

Both sides previous revisionPrevious revision
Next revision
Previous revision
cressington_sputter_coater_208hr [2015/08/10 07:55] steeniscressington_sputter_coater_208hr [2015/08/10 08:04] (current) steenis
Line 45: Line 45:
    - Replace glass cylinder and gently lower the top plate. Leave the system vented.    - Replace glass cylinder and gently lower the top plate. Leave the system vented.
  
-====== Manual process for Cr-sputtering =====+===== Manual process for Cr-sputtering =====
    - Select manual with the auto/manual button.    - Select manual with the auto/manual button.
    - Select timer for a timed process or MTM for a thickness controlled process.    - Select timer for a timed process or MTM for a thickness controlled process.
Line 68: Line 68:
  
 ====== Available Targets ====== ====== Available Targets ======
-^  Target Material  ^  Atomic Number  ^  Density in g/cm3  ^+^  Target Material  ^  Atomic Number  ^  Density in g/cm³  ^
 |  Pt/Pd (80/20)  |  78/46  |  19,52  | |  Pt/Pd (80/20)  |  78/46  |  19,52  |
 |  Cr  |  24  |  7,19  | |  Cr  |  24  |  7,19  |
cressington_sputter_coater_208hr.1439193311.txt.gz · Last modified: 2015/08/10 07:55 by steenis